Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.560 MPa-m/sec
16000 psi-ft/min
at 100 FPM, ambient temperature, thrust washer.
Techmer ES Plaslube® J-3/30/TF/13/SI/2 Nylon 6, 30% GFR, 13% PTFE, 2% Silicone
Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha..
Limiting Pressure Velocity 0.560 - 0.596 MPa-m/sec
16000 - 17000 psi-ft/min
Ensinger Tecast Vekton™ 6PALM Premium Bearing Grade cast nylon (PA6)
Tecast 6PALM contains both solid and liquid lubricants dispersed throughout the nylon to provide consistent wear rates and coefficients of friction.Information provided by Ensinger, Inc.
Limiting Pressure Velocity 0.560 MPa-m/sec
16000 psi-ft/min
at 1.27 m/s
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
Limiting Pressure Velocity 0.560 MPa-m/sec
16000 psi-ft/min
at 1.27 m/s
Cast Nylons Nycast® Nyloil® Lubricated Nylon
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
Limiting Pressure Velocity 0.560 MPa-m/sec
16000 psi-ft/min
at 1.27 m/s
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..