Polymer Property : Limiting Pressure Velocity = 0.596 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.560 - 0.596 MPa-m/sec
16000 - 17000 psi-ft/min
Ensinger Tecast Vekton™ 6PALM Premium Bearing Grade cast nylon (PA6)
Tecast 6PALM contains both solid and liquid lubricants dispersed throughout the nylon to provide consistent wear rates and coefficients of friction.Information provided by Ensinger, Inc.