Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 28.0 MPa | 4060 psi | ASTM D882 |
Eastman E6838-899F Polyethylene
(discontinued **) E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr.. |
|||
Film Tensile Strength at Yield, MD | 28.0 MPa @Temperature 23.0 °C |
4060 psi @Temperature 73.4 °F |
ASTM D638 |
Mapal Plastics Maplon PAPER MATCH Polypropylene Sheet Paper match is a multi layer graphic sheet. The core layer is a high rigidity PP. The skin layers are high field polyolefine. The surface bonds easily to inks and have some absorbing capacity.Main a.. |
|||
Film Tensile Strength at Yield, MD | 28.0 MPa | 4060 psi | ASTM D882 |
SCG Chemicals EL-Proâ„¢ P600F Polypropylene Film Resin Key Characteristics:Good optical propertiesHigh productivityGood openability with 3000 ppm slip agent and 2700 ppm antiblocking agentRecommended Applications:Water quenched blown film for food and a.. |
|||
Film Tensile Strength at Yield, MD | 28.0 MPa | 4060 psi | ASTM D882 |
SCG Chemicals EL-Proâ„¢ P602F Polypropylene Film Resin Key Characteristics:Excellent optical propertiesHigh productivityRecommended Applications:Water quenched blown film for food and apparel packagingCan be blended with P600 for excellent clarityInform.. |
|||
Film Tensile Strength at Yield, MD | 28.0 MPa | 4060 psi | ISO 527-3 |
EMS-Grivory Grivory® CR 8 PA* Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen.. |