Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, MD = 5.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 5.00 MPa
725 psi
ISO 527-3
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene
Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:..
Film Tensile Strength at Yield, MD 5.00 MPa
725 psi
ISO 527-3
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene
Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured..
Film Tensile Strength at Yield, MD 5.00 MPa
725 psi
ISO 527-3
Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene
Clearflex FF D0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FF D0 are highly transparent, have excellent sealing properties,..
Film Tensile Strength at Yield, MD 5.00 MPa
725 psi
ISO 527-3
Polimeri Europa Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FC 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FC 45 exhibit good optical properties, excellent impact resistance and low creep..
Film Tensile Strength at Yield, MD 5.00 MPa
725 psi
ISO 527-3
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex..
Film Tensile Strength at Yield, MD 5.00 MPa
725 psi
ASTM D882
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light..
Film Tensile Strength at Yield, MD 5.00 - 68.3 MPa
725 - 9910 psi
Average value: 12.5 MPa Grade Count:11
Overview of materials for Very Low Density Polyethylene (VLDPE)
This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va..
Film Tensile Strength at Yield, MD 5.00 - 44.0 MPa
725 - 6380 psi
Average value: 11.0 MPa Grade Count:120
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..