Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin
(discontinued **) Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1318CA Blown Film Resin
(discontinued **) Exceed 1318CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1318CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1518EC Tough Premium Film Resin
(discontinued **) Exceed 1518EC resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518EC resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018 DA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018 FA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 102.74 Thin Gauged Film Resin
(discontinued **) LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | ASTM D882 |
ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin Product Description: Exceed 1518HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | ASTM D882 |
ExxonMobil Exceed™ 1518KC Metallocene Polyethylene Resin Product Description: Exceed 1518KC is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518KC have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | ASTM D882 |
ExxonMobil Exceed™ 2018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018HA is a metallocene Catalyzed ethylene-hexene copolymer. Films made from Exceed 2018HA have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | ASTM D882 |
ExxonMobil Exceed™ 2018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018KB is a metallocene catalyzed ethylene-hexene copolymer. Films made from Exceed 2018KB have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 141.87 Shrink Film Resin LD 141.87 is a vinyl acetate copolymer film resin with very good toughness and shrink properties. Applications include Medium duty shrink wrap and Heavy duty bags.Information provided by ExxonMobil.. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | ASTM D882 |
ExxonMobil LDPE LGA 105 Low Density Polyethylene Resin Product Description: LGA 105 is a homopolymer, garment film resin with good toughness. It is capable of being draw-down to thin gauges.Availability: North America Additive: Antiblock: NoSlip: NoPro.. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | ASTM D882 |
Dow ELITE™ 5220G Enhanced Polyethylene Resin High impact and puncture resistance Excellent on-pallet load elongation for higher yields on regular loads Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018 EA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, MD | 8.96 MPa | 1300 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018 EB Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |