Polymer Property : Elmendorf Tear Strength MD = 440 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 440 g
440 g
ASTM D1922A
LyondellBasell Adflexâ„¢ Q 401 F TPO Resin
Thermoplastic olefin resin wit slip and antiblock for air quenched blown film, excellent heat resistance, excellent puncture resistance, great tear resistance, FDA acceptableApplications: films requ..
Elmendorf Tear Strength MD 440 g
440 g
ASTM D1922
Westlake Mxsten CV77529 Polyethylene Plastomer
Mxsten CV plastomer CV77529 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this ..
Elmendorf Tear Strength MD 440 g
440 g
ASTM D1922
ExxonMobil LDPE LGA 105 Low Density Polyethylene Resin
Product Description: LGA 105 is a homopolymer, garment film resin with good toughness. It is capable of being draw-down to thin gauges.Availability: North America Additive: Antiblock: NoSlip: NoPro..
Elmendorf Tear Strength MD 440 g
440 g
ASTM D1922
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin
Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell..