Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 8.0 g
8.0 g
Orientation not specified; ASTM D1922
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 150 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Elmendorf Tear Strength MD 8.0 g
8.0 g
ASTM D1922
Total HDPE HL 535 High Density Polyethylene, Film Resin
Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release ..
Elmendorf Tear Strength MD 8.0 g
8.0 g
ASTM D1922
ExxonMobil HDPE HTA 001HD High Density Polyethylene (HMW) Resin
Product Description: HTA 001HD is a high weight HDPE film grade. Films made from HTA 001HD exhibit excellent impact and toughness properties as well as high stiffness. Availability: Africa & Middle ..
Elmendorf Tear Strength MD 8.0 g
8.0 g
ASTM D1922
ExxonMobil HDPE HTA 002 High Density Polyethylene Resin
Product Description: HTA 002 is a general purpose medium molecular weight HDPE grade, characterized by easy processability, especially in coextrusion and blending with other polyolefins. HTA 002 can..
Elmendorf Tear Strength MD 8.0 g
8.0 g
ASTM D1922
Formosa Plastics Formolene® E927ND Film HDPE
High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E927ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi..