Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 150 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882
Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade
Homopolymer film gradeLow Residuals - Fina 3371 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor® 50 LBW OPP Film
Product Description: Bicor LBW is a two-sided treated, slip modified, non-heat sealable OPP film designed for use as the outside web of a lamination. The print surface is treated and can be printed ..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 120 XRG-2 OPP Film
Product Description: Bicor 120 XRG-2 is a one-side sealable OPP film that can be used as the inside web of a lamination where exceptional seal performance is required. The high-energy surface is int..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 70 XRG-2 OPP Film
Product Description: Bicor 70 XRG-2 is one-side treated, one-side sealable OPP film that can be used as the inside web of a lamination where exceptional seal performance is required. The high-energy..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Metallyte® 50 TSPM OPP Film
Product Description: A high barrier, non-sealable OPP film with one-side metalized a one-side treated. TSP< is designed for use as the inner web of a cold seal lamination or as the center web of a t..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Metallyte™ 12MM281 OPP Film
Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. 12MM281 is designed for use as the center web of a triplex adhesive lamination. The treated s..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST329 Polyester Film, 1000 Gauge
MELINEX® ST329 has good handling properties and a unique pearlescent appearance with no pre-treatments. It is heat stabilized for applications in high temperature processes where film registration ..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882A
DuPont Teijin Films Mylar® EB11 Polyester Film, 200 Gauge
Mylar® EB11 is a low gloss polyester film with a matte surface. It is typically used as a carrier film. It is commercially available in nominal 48 - 300 gauge. General Product Info: Mylar® EB11 is..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882A
DuPont Teijin Films Mylar® EB11 Polyester Film, 300 Gauge
Mylar® EB11 is a low gloss polyester film with a matte surface. It is typically used as a carrier film. It is commercially available in nominal 48 - 300 gauge. General Product Info: Mylar® EB11 is..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882A
DuPont Teijin Films Mylar® EB11 Polyester Film, 92 Gauge
Mylar® EB11 is a low gloss polyester film with a matte surface. It is typically used as a carrier film. It is commercially available in nominal 48 - 300 gauge. General Product Info: Mylar® EB11 is..
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882A
DuPont Teijin Films Mylar® EB11 Polyester Film, 48 Gauge
Mylar® EB11 is a low gloss polyester film with a matte surface. It is typically used as a carrier film. It is commercially available in nominal 48 - 300 gauge. General Product Info: Mylar® EB11 is..