Film Tensile Strength at Break, MD 26.5 MPa
3840 psi
500mm/min, Ultimate; ASTM D638
LG Chemical SEETEC BF315 LDPE
Characteristics: Good Processability and Excellent Optical PropertiesApplications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical
Film Tensile Strength at Break, MD 26.5 MPa
3840 psi
500mm/min, Ultimate; ASTM D638
LG Chemical SEETEC BF410 LDPE
Characteristics: Good Processability and Excellent Optical PropertiesAdditives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG ..
Film Tensile Strength at Break, MD 26.5 MPa
3840 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF200GG Low density polyethylene
LDF200GG is a low density polyethylene resin for film extrusion. LDF200GG has medium slip and anti-block additives. LDF200GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta..
Film Tensile Strength at Break, MD 26.5 MPa
3840 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene
LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
Film Tensile Strength at Break, MD 26.5 MPa
3840 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF201FG Low density polyethylene
LDF201FG is a low density polyethylene resin for film extrusion. LDF201FG has low slip and anti-block additives. LDF201FG meets the U.S. Food and Drug Administration (FDA) criteria for food contact ..