LG Chemical SEETEC BF410 LDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LG Chemical
Trade Name SEETEC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC BF410 LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Good Processability and Excellent Optical PropertiesAdditives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.922 - 0.926 g/cc
0.922 - 0.926 g/cc
ASTM D1505
Melt Flow 1.8 - 2.0 g/10 min

@Load 2.61 kg,
Temperature 190 °C
1.8 - 2.0 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.2 MPa
1920 psi
500mm/min; ASTM D638
Film Elongation at Break, MD 300 %
300 %
500 mm/min; ASTM D638
Film Elongation at Break, TD 550 %
550 %
500 mm/min; ASTM D638
Elongation at Break 650 %
650 %
500 mm/min; ASTM D638
2% Secant Modulus 1.35 GPa
196 ksi
500mm/min; ASTM D638
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
Dart Drop Test 65.0 g
0.143 lb
ASTM D1709
Film Tensile Strength at Break, MD 26.5 MPa
3840 psi
500mm/min, Ultimate; ASTM D638
Film Tensile Strength at Break, TD 23.5 MPa
3410 psi
500mm/min, Ultimate; ASTM D638
Thermal Properties Metric English Comments
Melting Point 107 °C
225 °F
10°C/min; ASTM D3418
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 4.0 %
4.0 %
ASTM D1003
Gloss 95 %
95 %
45°; ASTM D2457