Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ISO 527
Premix Thermoplastics PRE-ELEC® CP 1317
PRE-ELEC CP 1317 is a conductive thermoplastic compound based on EVA. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC CP 1317 ..
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ISO 527
Premix Thermoplastics PRE-ELEC® CP 1319
PRE-ELEC CP 1319 is a conductive thermoplastic compound based on EVA. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC CP 1319 ..
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ASTM D882
Westlake EMAC® SP2242 Specialty Copolymer  (discontinued **)
EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo..
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ASTM D882
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process..
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ASTM D882
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es..
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ASTM D882
Huntsman PE1055 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Yields film with excellent optical and draw down characteristicsApplications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms..
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ASTM D882
Huntsman PE1080 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrapFDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under..
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ASTM D882
Huntsman PE 1402 EVA Film Extrusion  (discontinued **)
4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Copyright © lookpolymers.com All Rights Reserved