Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.10 - 66.4 MPa | 160 - 9630 psi | Average value: 14.1 MPa Grade Count:181 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Tensile Strength, Yield | 1.10 MPa | 160 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-530 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.10 MPa @Strain 100 % |
160 psi @Strain 100 % |
ASTM D412 |
Multibase Multi-Flex® A 5001 E LC Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase |
|||
Tensile Strength, Yield | 1.10 MPa | 160 psi | 100%; ASTM D412 |
Multibase Multi-Flex® A 5001 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, GoodWe.. |
|||
Tensile Strength, Yield | >= 1.10 MPa | >= 160 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5353 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.10 MPa | 159 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7189 Ethylene-Propylene Rubber General service EPDMInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.10 MPa | 160 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7284 Butyl and Halobutyl Rubber Chlorobutyl; High damping; Non-conductiveInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.10 MPa | 160 psi | at 150% elongation, maximum |
Dow Corning 3-0105 AUTOMOTIVE SEALANT One-part RTV, alkoxy cure, designed for automotive powertrain sealing applicationsInformation provided by Dow Corning |