Polymer Property : Tensile Strength, Yield = 160 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.10 - 66.4 MPa
160 - 9630 psi
Average value: 14.1 MPa Grade Count:181
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Tensile Strength, Yield 1.10 MPa
160 psi
200%, post cured- 8 hours at 177°C; ASTM D412
Multibase C6-530 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.10 MPa

@Strain 100 %
160 psi

@Strain 100 %
ASTM D412
Multibase Multi-Flex® A 5001 E LC Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase
Tensile Strength, Yield 1.10 MPa
160 psi
100%; ASTM D412
Multibase Multi-Flex® A 5001 LC TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, GoodWe..
Tensile Strength, Yield >= 1.10 MPa
>= 160 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 5353 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 1.10 MPa
160 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7284 Butyl and Halobutyl Rubber
Chlorobutyl; High damping; Non-conductiveInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 1.10 MPa
160 psi
at 150% elongation, maximum
Dow Corning 3-0105 AUTOMOTIVE SEALANT
One-part RTV, alkoxy cure, designed for automotive powertrain sealing applicationsInformation provided by Dow Corning