Mechanical Properties Metric English Comments
Tensile Strength, Yield 731 MPa
106000 psi
Kinetics MIM 17-4PH Stainless Steel (As Sintered)
Precipitation-hardening stainless steel. Offers a good balance between corrosion resistance and strength. Magnetic. Hardenable to various strength levels and hardness by varying the aging heat treat..
Tensile Strength, Yield >= 730 MPa

@Strain 0.200 %,
Diameter 9.52 mm
>= 106000 psi

@Strain 0.200 %,
Diameter 0.375 in
CWSR; DAN 2700.9
Haynes Ti-3Al-2.5V Alloy Titanium Tubing
Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani..
Tensile Strength, Yield >= 730 MPa

@Diameter 12.7 - 25.4 mm,
Strain 0.200 %
>= 106000 psi

@Diameter 0.500 - 1.00 in,
Strain 0.200 %
CWSR; DAN 2700.9
Haynes Ti-3Al-2.5V Alloy Titanium Tubing
Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani..
Tensile Strength, Yield 730 MPa

@Strain 0.200 %
106000 psi

@Strain 0.200 %
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 731 MPa
106000 psi
HP Alloys Alloy X, 15% Cold Worked
15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International.