Polymer Property : Tensile Strength, Yield = 731 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 731 MPa
106000 psi
Kinetics MIM 17-4PH Stainless Steel (As Sintered)
Precipitation-hardening stainless steel. Offers a good balance between corrosion resistance and strength. Magnetic. Hardenable to various strength levels and hardness by varying the aging heat treat..
Tensile Strength, Yield 731 MPa
106000 psi
HP Alloys Alloy X, 15% Cold Worked
15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International.