Material Notes:
Precipitation-hardening stainless steel. Offers a good balance between corrosion resistance and strength. Magnetic. Hardenable to various strength levels and hardness by varying the aging heat treat temperature. Typically provides better corrosion resistance than the 400 series stainless steels, and better strength than the 300 series stainless steels. Often used for aircraft, dental, marine, medical, surgical, and applications where high levels of strength and hardness, and good corrosion resistance is requiredProperty values reported are typical for Kinetics' MIM products.Metal Injection Molding General Notes: Fine metal powders (generally
Physical Properties Metric English Comments
Density 7.60 g/cc
0.275 lb/in³
Sintered
Mechanical Properties Metric English Comments
Hardness, Rockwell C 27
27
Tensile Strength, Ultimate 896 MPa
130000 psi
Tensile Strength, Yield 731 MPa
106000 psi
Elongation at Break 9.0 %
9.0 %
in 1 inch
Reduction of Area 38 %
38 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.070 %
<= 0.070 %
Chromium, Cr 15.5 - 17.5 %
15.5 - 17.5 %
Copper, Cu 3.0 - 5.0 %
3.0 - 5.0 %
Iron, Fe 70 - 78.4 %
70 - 78.4 %
by difference
Manganese, Mn <= 1.0 %
<= 1.0 %
Nb + Ta 0.15 - 0.45 %
0.15 - 0.45 %
Nickel, Ni 3.0 - 5.0 %
3.0 - 5.0 %
Silicon, Si <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Surface Finish 30 Ra