Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.86 MPa | 1140 psi | ASTM D412 |
Teknor Apex APEX® 1700-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met.. |
|||
Tensile Strength, Yield | 7.86 MPa | 1140 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SHM 6200 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 7.86 MPa | 1140 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SFW 10500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Uses: Footwear; General Purpose Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 7.85 MPa | 1140 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® X-590A-2FR Thermoplastic Polyurethane Type: Estane® X-590A-2FR TPU is a Shore 89A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Tensile Strength, Yield | 7.85 MPa | 1140 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® R180A Thermoplastic Polyurethane Type: Estane® R180A is a Shore 83A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |