Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.85 MPa
1140 psi
at 100% elongation; ASTM D412
Lubrizol Estane® X-590A-2FR Thermoplastic Polyurethane
Type: Estane® X-590A-2FR TPU is a Shore 89A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation
Tensile Strength, Yield 7.85 MPa
1140 psi
at 300% elongation; ASTM D412
Lubrizol Estane® R180A Thermoplastic Polyurethane
Type: Estane® R180A is a Shore 83A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi..
Copyright © lookpolymers.com All Rights Reserved