Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 143 MPa | 20700 psi | ASTM D638 |
LNP Thermotuf® OF-1006 HI Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades .. |
|||
Tensile Strength, Yield | 143 MPa | 20700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 143 MPa | 20700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 143 MPa | 20700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Tensile Strength, Yield | 143 MPa | 20700 psi | ASTM D638 |
LNP Thermocomp® JF-1006 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Tensile Strength, Yield | 143 MPa | 20700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |