Polymer Property : Tensile Strength, Yield = 155900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1075 MPa
155900 psi
Industeel Superplast® 400 High Hardness Mold Steel
SUPERPLAST® 400 is an injection plastic mold steel pre-hardened to a high level of hardness. It is delivered at a typical hardness of 125 kg/mm2. This steel is specially adapted for heavy-duty ..
Tensile Strength, Yield 1075 MPa

@Strain 0.200 %
155900 psi

@Strain 0.200 %
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Fastener Stock
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of fastener stock; more specific form/thickness entries are also available in MatWeb.Industry Specifications: ..
Tensile Strength, Yield 1075 MPa

@Strain 0.200 %
155900 psi

@Strain 0.200 %
Haynes 556® alloy, 40% cold reduction
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..