Industeel Superplast® 400 High Hardness Mold Steel

Category Metal , Ferrous Metal , Alloy Steel , Tool Steel , Mold Steel
Manufacturer Groupe Arcelor
Trade Name Superplast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel Superplast® 400 High Hardness Mold Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SUPERPLAST® 400 is an injection plastic mold steel pre-hardened to a high level of hardness. It is delivered at a typical hardness of 125 kg/mm2. This steel is specially adapted for heavy-duty molds used for production of long series, for compression molds or when an improved wear resistance is expected. SUPERPLAST® 400 will be ideal where a high resistance of the mating plan surface is required and when the conventional 300 HB or even conventional high hard material cannot ensure adapted properties. SUPERPLAST® 400 exhibits processing aptitudes strongly improved compared to conventional steel W1.2711 or equivalent, heat treated to same hardness. This improvement mainly results from a new chemical balance. SUPERPLAST® 400, delivered at 350 to 380 HB, has excellent weldability, a better micro structural homogeneity and a much better machinability than conventional grades heat treated to the same level or even lower hardness.All injection molds demanding high mechanical properties: long series; high injection series; injection of reinforced plastics (glass fibers); wear problems; compression molds
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 360
360
Tensile Strength, Ultimate 1250 MPa
181000 psi
Tensile Strength, Yield 1075 MPa
155900 psi
Elongation at Break >= 10 %
>= 10 %
Modulus of Elasticity 210 GPa
30500 ksi
Thermal Properties Metric English Comments
CTE, linear 10.8 µm/m-°C

@Temperature 20.0 - 100 °C
6.00 µin/in-°F

@Temperature 68.0 - 212 °F
11.2 µm/m-°C

@Temperature 20.0 - 200 °C
6.22 µin/in-°F

@Temperature 68.0 - 392 °F
12.9 µm/m-°C

@Temperature 20.0 - 300 °C
7.17 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 38.0 W/m-K
264 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.30 %
<= 0.30 %
Chromium, Cr 2.0 %
2.0 %
Iron, Fe >= 94.9 %
>= 94.9 %
Manganese, Mn 1.15 %
1.15 %
Molybdenum, Mo 0.65 %
0.65 %
Nickel, Ni 1.0 %
1.0 %
Sulfur, S <= 0.020 %
<= 0.020 %