Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Nylene® PA6 Glass Filled 5233 HS Nylon 6 33% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | 5 nm; ISO 527-2/1A/5 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Nymax™ GF1800-40 HS Black 13 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedHeat StabilizedNylon 6/12 CompoundBlackDry as molded:PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 162 MPa @Thickness 3.20 mm |
23500 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Tensile Strength, Yield | 162 MPa @Thickness 3.20 mm |
23500 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 162 MPa @Thickness 3.20 mm |
23500 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA 6/10 (Asia Pacific) LNP* Lubricomp* QCL349 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, Flame Retardant, Elect.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Tensile Strength, Yield | 162 MPa @Thickness 5.00 mm |
23500 psi @Thickness 0.197 in |
5 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF30 FR NAT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF33 FR-N BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF30 L X MT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: SilverTPCI# 7210102Information provid.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF40 A1 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: Lubricated, Low Shrinkage and Good Wear ResistanceAppearan.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 UG BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Samyang Tripet® 2500G30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 03004 GF20 Carbon/20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement/Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatu.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Cheng Yu Plastic N6G10 Nylon 6, 10% Glass Filled |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Ashley Polymers Ashlene® E128 PET Polyester, 45% Glass Reinforced PET Polyester, economy grade with 45% glass reinforcement.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced 6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 33% Glass Reinforced.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66 Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10 LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti.. |
|||
Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF30 FR HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |