Polymer Property : Tensile Strength, Yield = 17500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 - 121 MPa
16000 - 17500 psi
Average value: 115 MPa Grade Count:5
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea..
Tensile Strength, Yield 35.0 - 121 MPa
5080 - 17500 psi
Average value: 81.1 MPa Grade Count:24
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Tensile Strength, Yield 40.7 - 121 MPa
5900 - 17500 psi
Average value: 62.8 MPa Grade Count:27
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..