Polymer Property : Tensile Strength, Yield = 184 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 184 MPa
26700 psi
5.0 mm/min; ISO 527
PolyOne Nymax™ GF 1200 A 33 HS Black 22 Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Tensile Strength, Yield 184 MPa
26700 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66
Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 184 MPa
26700 psi
ISO 527-2
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM
Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..