Tensile Strength, Yield 19.0 - 21.4 MPa
2760 - 3100 psi
Average value: 20.5 MPa Grade Count:3
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..