Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.45 MPa
210 psi
at 200%, post cured- 2 hours at 177°C
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.45 MPa
210 psi
at 200%, as molded
Multibase SILASTIC® C7-4535 VAROX Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.45 MPa
210 psi
at 100%; ASTM D412
PB1100-60 Polyurethane-based Biomedical Elastomer
Tensile Strength, Yield 1.45 MPa
210 psi
200%, post cured- 4 hours at 177°C; ASTM D412
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.45 MPa
210 psi
at 200%, post cured- 2 hours at 177°C; ASTM D412
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.45 MPa
210 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7075 Ethylene-Propylene Rubber