Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.2 MPa | 3800 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ DP-9162-3 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP FR 7B31 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | 2 in per min, tangent; ASTM D638 |
Network Polymers NPP 20-1001 Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | Type 1 bar; ASTM D638 |
Network Polymers Softflex® UB 30 Black OEX Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Petromont 4101 High Density Polyethylene Resin Petromont HDPE 4101 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is primarily used in the extrusion of corrugated pipes for drainage applications, f.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 0 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with DOP Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Flint Hills 43S2A Polypropylene Random Copolymer Features: Good clarity.Applications: Film extrusion and blow moldingInformation Provided by Flint Hills Resources |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | 2 in/min (50 mm/min); ASTM D-638 |
Ineos G50-100 HDPE Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding p.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Techmer ES HiFill® PP 0202 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Techmer ES HiFill® PP 0254 S Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Techmer ES HiFill® PP 0254 S1 003 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Good Corrosion ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Techmer ES HiFill® PP GB20 20% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | >= 26.2 MPa | >= 3800 psi | ASTM D 638 type IV |
Total 50100.1 HDPE blow molding Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging. Blow Molding Stock Temperature 370 – 450 ºF Extrusion melt tempera.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with DOP Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 0 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | >= 26.2 MPa | >= 3800 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
CPC - Vycom PROTEC® Copolymer Polypropylene (CPP) Protec CP is one of various types of "impact copolymers"—a rapidly growing segment of the thermoplastic sheet market. In contrast to homopolymer polypropylene (which involves the polymerization of .. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
ExxonMobil HDPE HD 6704.18 High Density Polyethylene Copolymer Resin Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | 2 in/min; ASTM D638 |
ExxonMobil HDPE HYA 600 High Density Polyethylene Resin Product Description: HYA 600 is a general purpose HDPE resin, characterized by very easy processability, an excellent balance of rigidity and impact strength and a good ESCR.Availability: Africa & M.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
ExxonMobil Paxon™ BA50-100 Blow Molding Resin Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
ExxonMobil HD 6706.17 Injection Molding Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
ExxonMobil HD 6706.62 Injection Molding Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM Data |
Dow Retain® PS-4000 Polystyrene Data provided by Dow Chemical. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow UNIVAL™ DMDD-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6200 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package hous.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Lubrizol Stat-Rite® M-809 Static Control Acrylic Stat-Rite® M-809 is a static dissipative Acrylic alloy. Stat-Rite® M-809 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protec.. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D882 |
Formosa Plastics Formolene® LH5204 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, lids and over-capsFormolene LH5204 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as .. |
|||
Tensile Strength, Yield | 26.2 MPa | 3800 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 33% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |