Total 50100.1 HDPE blow molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Total Atofina
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total 50100.1 HDPE blow molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging. Blow Molding Stock Temperature 370 – 450 ºF Extrusion melt temperature 380 - 480ºFInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D 792
Environmental Stress Crack Resistance >= 600 hour
>= 600 hour
ASTM D1693 cond. B 100% lgepal
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 26.2 MPa
>= 3800 psi
ASTM D 638 type IV
Elongation at Break 600 %
600 %
ASTM D 638, type IV
Flexural Modulus 1.21 GPa
175 ksi
ASTM D 790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 127 °C
260 °F
ASTM D3417