Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.99 MPa
3045 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 20.99 MPa
3045 psi
50 mm/min; ASTM D638
ICO Polymers ICORENEâ„¢ 150-1335 LMDPE Rotational Molding Resin
Description: ICORENE 150-1335 is a linear medium density polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good proce..
Tensile Strength, Yield 20.99 MPa
3045 psi
50 mm/min; ASTM D638
ICO Polymers ICORENEâ„¢ 155-1330 LMDPE Rotational Molding Resin
Description: ICORENE 155-1330 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi..
Tensile Strength, Yield 20.99 MPa
3045 psi
50 mm/min; ASTM D638
ICO Polymers ICORENEâ„¢ 195-1330 LMDPE Rotational Molding Resin
Description: ICORENE 195-1330 is a compounded linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and sti..
Tensile Strength, Yield 20.99 MPa
3045 psi
50 mm/min; ASTM D638
ICO Polymers ICORENEâ„¢ 195-1336 LMDPE Rotational Molding Resin
Description: ICORENE 195-1336 is a compounded linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and sti..
Tensile Strength, Yield 20.99 MPa
3045 psi
At 50 mm/min; ISO 527-2
Borealis Borsoft™ SE410MO Polypropylene for Injection Molding
Borsoft SE410MO is a specially designed modified relatively soft polypropylene heterophasic copolymer with medium melt flow intended for injection moldingBorsoft SE410MO is a tailor made grade desig..
Tensile Strength, Yield 20.99 MPa
3045 psi
At 50 mm/min; ISO 527-2
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled
Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i..
Tensile Strength, Yield 20.99 MPa
3045 psi
At 50 mm/min; ISO 527-2
Borealis Daplen™ KSR65T20 Polypropylene Compound 20% Mineral Filled
Daplen KSR65T20 is a 20% mineral filled grade for injection molding. Daplen KSR65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSR65T20 offers very g..
Tensile Strength, Yield 20.99 MPa
3045 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..