Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 33.9 MPa | 4920 psi | ASTM D638 |
Spartech Royalite R21M General Purpose ABS Resin Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta.. |
|||
Tensile Strength, Yield | 33.9 MPa | 4920 psi | 81% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 33.9 MPa | 4920 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers DIAMALOY WPE 2000 Wood Filled HDPE Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 33.9 MPa | 4920 psi | ASTM D638 |
Cheng Yu Plastic BK1020 Electric Conducting LDPE |