Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers DIAMALOY WPE 2000 Wood Filled HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Wood Filled
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY WPE 2000 Wood Filled HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Melt Flow 0.10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
23.6 g/10 min

@Load 2.16 kg,
Temperature 230 °C
23.6 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.9 MPa
4920 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 8.7 %
8.7 %
chs 2.0 in/min; ASTM D638
Flexural Strength 29.8 MPa
4320 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 1.123 GPa
162.9 ksi
chs 0.05 in/min; ASTM D790