Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.9 MPa
4920 psi
ASTM D638
Spartech Royalite R21M General Purpose ABS Resin
Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta..
Tensile Strength, Yield 33.9 MPa
4920 psi
81% Ret.
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 33.9 MPa
4920 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers DIAMALOY WPE 2000 Wood Filled HDPE
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 33.9 MPa
4920 psi
ASTM D638
Cheng Yu Plastic BK1020 Electric Conducting LDPE