Tensile Strength, Yield 105 - 234 MPa
15200 - 34000 psi
Average value: 180 MPa Grade Count:55
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Tensile Strength, Yield 29.0 - 234 MPa
4200 - 34000 psi
Average value: 104 MPa Grade Count:192
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..