Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 280 - 350 MPa

@Strain 0.200 %
40600 - 50800 psi

@Strain 0.200 %
SSAB Tunnplat Aluzink 280A YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is ..
Tensile Strength, Yield 280 - 350 MPa

@Strain 0.200 %
40600 - 50800 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 280YP High-strength Steel
High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report..
Tensile Strength, Yield 280 - 350 MPa

@Strain 0.200 %
40600 - 50800 psi

@Strain 0.200 %
SSAB Tunnplat Dogal 280YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur..
Tensile Strength, Yield 250 - 350 MPa

@Strain 0.200 %
36300 - 50800 psi

@Strain 0.200 %
CLAL-MSX NICLAL 3444 H12 1/2 Hard Copper Alloy, Free Cutting Bronze
Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b..