Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 40600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 280 MPa

@Strain 0.200 %,
Temperature 538 °C
40600 psi

@Strain 0.200 %,
Temperature 1000 °F
Kennametal Stellite Stellite® 31 PM cast
Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we..
Tensile Strength, Yield 280 - 720 MPa

@Strain 0.200 %
40600 - 104000 psi

@Strain 0.200 %
Materion Brush 1915â„¢ Annealed Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %
40600 psi

@Strain 0.200 %
Annealed prior to test
Special Metals INCOLOY® Alloy 330
A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospher..
Tensile Strength, Yield 280 - 350 MPa

@Strain 0.200 %
40600 - 50800 psi

@Strain 0.200 %
SSAB Tunnplat Aluzink 280A YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is ..
Tensile Strength, Yield 280 - 350 MPa

@Strain 0.200 %
40600 - 50800 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 280YP High-strength Steel
High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report..
Tensile Strength, Yield 280 - 450 MPa

@Strain 0.200 %
40600 - 65300 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 600DL High-strength Steel
High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact..
Tensile Strength, Yield >= 280 MPa

@Strain 0.200 %
>= 40600 psi

@Strain 0.200 %
SSAB Tunnplat Docol® DC01 (Fe P01) Deep-drawing Steel
Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported by the manufacturer...
Tensile Strength, Yield 280 - 350 MPa

@Strain 0.200 %
40600 - 50800 psi

@Strain 0.200 %
SSAB Tunnplat Dogal 280YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur..
Tensile Strength, Yield >= 280 MPa
>= 40600 psi
SSAB Tunnplat Domex® 280XP Extra High-strength Cold-forming Steel
Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene..
Tensile Strength, Yield >= 280 MPa
>= 40600 psi
SSAB Tunnplat Domex® 280YP Cold-forming Steel, HSLA
Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®..
Tensile Strength, Yield 280 MPa
40600 psi
90º, RT, Dry; EN2561
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 63%/120 E-Glass Fiber
Information provided by HexCel
Tensile Strength, Yield 280 MPa
40600 psi
As Cast
AFE Technologies Cronite 25Cr/12Ni No. HR7
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..
Tensile Strength, Yield >= 280 MPa
>= 40600 psi
AK Steel ASTM A 463 / SAE J1392 040 AHK, Grade 40 Aluminized Carbon Steel, Structural Steel (SS)
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel
Tensile Strength, Yield >= 280 MPa
>= 40600 psi
AK Steel SAE J1392 040XLK or 040YLK, Grade 40 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS)
Information provided by AK Steel
Tensile Strength, Yield >= 280 MPa
>= 40600 psi
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, HSLAS, FORMABLE 40K / SAE J1392 040 XLK or 040 YLK
Information provided by AK Steel
Tensile Strength, Yield >= 280 MPa
>= 40600 psi
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 040XLK
SAE Specified properties not covered by ASTMInformation provided by AK Steel
Tensile Strength, Yield 280 - 340 MPa
40600 - 49300 psi
ArcelorMittal Dual Phase 450 Very high strength steel, Cold Rolled Steel
Available in the following: HCT500X (uncoated), HCT500X+ZE (electrogalvanized) and HCT500X+Z (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength and ..
Tensile Strength, Yield 280 MPa

@Strain 0.200 %,
Temperature 538 °C
40600 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Tensile Strength, Yield 280 MPa

@Strain 1.00 %
40600 psi

@Strain 1.00 %
Typical after Solution Annealing
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants
Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum..
Copyright © lookpolymers.com All Rights Reserved