SSAB Tunnplat Aluzink 280A YP High-strength Metal-coated Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer SSAB Tunnplat AB
Trade Name Aluzink
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Aluzink 280A YP High-strength Metal-coated Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 350 - 420 MPa
50800 - 60900 psi
Tensile Strength, Yield 280 - 350 MPa

@Strain 0.200 %
40600 - 50800 psi

@Strain 0.200 %
Elongation at Break >= 24 %
>= 24 %
A<sub>80</sub>; For thicknesses < 0.70 mm values 2% lower apply
Bend Radius, Minimum >= 1.0 t
>= 1.0 t
90° bending; avoid bending and rebending
Component Elements Properties Metric English Comments
Iron, Fe 98 %
98 %