Polymer Property : Tensile Strength, Yield = 379 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 276 - 379 MPa

@Strain 0.200 %
40000 - 55000 psi

@Strain 0.200 %
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast & Aged)
Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr..
Tensile Strength, Yield 241 - 379 MPa

@Strain 0.200 %,
Thickness >=25.4 mm
35000 - 55000 psi

@Strain 0.200 %,
Thickness >=1.00 in
Turned Bars
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar
Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros..
Tensile Strength, Yield 241 - 379 MPa

@Strain 0.200 %,
Thickness >=25.4 mm
35000 - 55000 psi

@Strain 0.200 %,
Thickness >=1.00 in
Turned Bars
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar
Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre..
Tensile Strength, Yield 317 - 379 MPa
46000 - 55000 psi
0.2% offset
Eagle Brass 110 EPT COPPER, Extra Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Tensile Strength, Yield 310 - 379 MPa
45000 - 55000 psi
0.2% offset
Eagle Brass 210 Gilding Metal, 3/4 Hard
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
Tensile Strength, Yield 276 - 379 MPa
40000 - 55000 psi
0.2% offset
Eagle Brass 519 Phosphor Bronzes 6%, 1/4 Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
Tensile Strength, Yield 317 - 379 MPa
46000 - 55000 psi
0.2% offset
Eagle Brass 101 OFE COPPER (Certified), Extra Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Tensile Strength, Yield 317 - 379 MPa
46000 - 55000 psi
0.2% offset
Eagle Brass 102 OF COPPER (Non-Certified), Extra Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Tensile Strength, Yield 172 - 379 MPa

@Strain 0.200 %
24900 - 55000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899A 1/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 172 - 379 MPa

@Strain 0.200 %
24900 - 55000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899L 1/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 172 - 379 MPa

@Strain 0.200 %
24900 - 55000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899M 1/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 310 - 379 MPa

@Strain 0.200 %
45000 - 55000 psi

@Strain 0.200 %
Annealed
AK Steel 15 Cr-Cb® ULTRA FORM® Ferritic Stainless steel
AK Steel’s 15 Cr-Cb ULTRA FORM® is a low-carbon, low-nitrogen ferritic grade of stainless steel with an intermediate, 14.5% chromium content. Alloying additions of Ti, Cb, Si and Mn provide excell..