Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 39.3 - 40.7 MPa | 5700 - 5900 psi | Average value: 40.1 MPa Grade Count:7 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Yield | 24.1 - 40.7 MPa | 3500 - 5900 psi | Average value: 34.9 MPa Grade Count:78 |