Tensile Strength, Yield 29.3 MPa
4250 psi
ASTM D638
Omni Plastics OmniTuff™ CPP TF30 Copolymer Polypropylene Talc Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Tensile Strength, Yield 29.3 MPa
4250 psi
(2 in/min); ASTM D638
Phillips 66 COPYLENE® CR350CS-01 Polypropylene Random Copolymer
COPYLENE® CR350CS-01 is a clarified, reactor grade, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release for larger ar..
Tensile Strength, Yield 29.3 MPa
4250 psi
aged 96 hours at 158ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tensile Strength, Yield 29.3 MPa
4250 psi
50 mm/min; ASTM D638
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade
ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case..
Tensile Strength, Yield 29.3 MPa
4250 psi
ASTM D638
Ineos R55C-00 Clarified Polypropylene Copolymer
Grade R55C-00 is a high melt flow rate clarified and antistatic random polypropylene copolymer. It is designed for high speed injection molding of thin walled parts requiring very good mold filling ..
Tensile Strength, Yield 29.3 MPa
4250 psi
2 in/min; ASTM D638
Ineos R05C-00 Polypropylene Random Copolymer
Random copolymer R05C-00 is an antistatic, clarified polypropylene random copolymer produced by a unique catalyst technology. It is designed as a high gloss resin and exhibits good stiffness and imp..
Tensile Strength, Yield 29.3 MPa
4250 psi
2"/min; ASTM D638
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Tensile Strength, Yield 29.3 MPa
4250 psi
70% Ret.
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 29.3 MPa
4250 psi
2"/min; ASTM D638
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Tensile Strength, Yield 29.3 MPa
4250 psi
2"/min; ASTM D638
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Tensile Strength, Yield 29.3 MPa
4250 psi
2"/min; ASTM D638
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Tensile Strength, Yield 29.3 MPa
4250 psi
70% Ret.
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 29.3 MPa
4250 psi
2"/min; ASTM D638
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Tensile Strength, Yield 29.3 MPa
4250 psi
aged 96 hours at 158ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tensile Strength, Yield 29.3 MPa
4250 psi
2"/min; ASTM D638
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Tensile Strength, Yield 29.3 MPa
4250 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 29.3 MPa
4250 psi
ASTM D638
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Tensile Strength, Yield 29.3 MPa
4250 psi
ASTM D638
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Tensile Strength, Yield 29.3 MPa
4250 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..