Ineos R05C-00 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos R05C-00 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Random copolymer R05C-00 is an antistatic, clarified polypropylene random copolymer produced by a unique catalyst technology. It is designed as a high gloss resin and exhibits good stiffness and improved cycle time. Product grade R05C-00 meets FDA requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.898 g/cc
0.0324 lb/in³
ASTM D1505
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength at Break 18.6 MPa
2700 psi
2 in/min; ASTM D638
Tensile Strength, Yield 29.3 MPa
4250 psi
2 in/min; ASTM D638
Elongation at Break 550 %
550 %
2 in/min; ASTM D638
Elongation at Yield 10 %
10 %
2 in/min; ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
1% Secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.427 J/cm

@Diameter 3.17 mm
0.800 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Izod Impact, Unnotched >= 13.3 J/cm
>= 25.0 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved