Polymer Property : Tensile Strength, Yield = 455 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 372 - 455 MPa
54000 - 66000 psi
0.2% offset
Eagle Brass 19210 XP-10 Copper Iron, Hard
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Tensile Strength, Yield 352 - 455 MPa
51000 - 66000 psi
0.2% offset
Eagle Brass 425 Tin Brass 2%, 1/2 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Yield 172 - 455 MPa
25000 - 66000 psi
Chicago Extruded Metals BioBrass® UNS C46400 Copper-Zinc-Tin Alloy
Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, wire, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Met..