Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 269 - 331 MPa | 39000 - 48000 psi | 0.2% offset |
Eagle Brass 110 EPT COPPER, 3/4 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Yield | 159 - 331 MPa | 23000 - 48000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, 1/4 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | 269 - 331 MPa | 39000 - 48000 psi | 0.2% offset |
Eagle Brass 101 OFE COPPER (Certified), 3/4 Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Yield | 269 - 331 MPa | 39000 - 48000 psi | 0.2% offset |
Eagle Brass 102 OF COPPER (Non-Certified), 3/4 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Yield | 296 - 331 MPa @Strain 0.200 % |
42900 - 48000 psi @Strain 0.200 % |
|
AK Steel 439 Ferritic Stainless steel AK Steel 439 has better oxidation and corrosion resistance than Type 409. This alloy also has optimum formability that is reproducible coil after coil and heat after heat. This provides special ad.. |
|||
Tensile Strength, Yield | 276 - 331 MPa @Strain 0.200 %, Thickness 1.02 - 1.78 mm |
40000 - 48000 psi @Strain 0.200 %, Thickness 0.0402 - 0.0701 in |
|
AK Steel 439 LT Ferritic Stainless steel AK Steel 439 LT has oxidation and corrosion resistance comparable to Type 439 stainless steel. This alloy also has optimum formability that is reproducible coil after coil and heat after heat. Thi.. |