AK Steel 439 LT Ferritic Stainless steel

Category Metal , Ferrous Metal , Ferritic , Stainless Steel , T 400 Series Stainless Steel
Manufacturer AK Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel 439 LT Ferritic Stainless steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AK Steel 439 LT has oxidation and corrosion resistance comparable to Type 439 stainless steel. This alloy also has optimum formability that is reproducible coil after coil and heat after heat. This provides special advantages when producing difficult-to-form exhaust system components. The lower titanium content of AK Steel 439 LT Stainless Steel provides an improved surface free from titanium scale.Information provided by AK Steel
Mechanical Properties Metric English Comments
Hardness, Rockwell B 73 - 79

@Thickness 1.02 - 1.78 mm
73 - 79

@Thickness 0.0402 - 0.0701 in
Tensile Strength, Ultimate 442 - 497 MPa

@Thickness 1.02 - 1.78 mm
64100 - 72100 psi

@Thickness 0.0402 - 0.0701 in
Tensile Strength, Yield 276 - 331 MPa

@Strain 0.200 %,
Thickness 1.02 - 1.78 mm
40000 - 48000 psi

@Strain 0.200 %,
Thickness 0.0402 - 0.0701 in
Elongation at Break 30 - 35 %
30 - 35 %
in 2 inches (1.02 - 1.78 mm)
Component Elements Properties Metric English Comments
Carbon, C <= 0.025 %
<= 0.025 %
Chromium, Cr 17 - 19 %
17 - 19 %
Iron, Fe >= 78.725 %
>= 78.725 %
As Remainder
Manganese, Mn <= 0.50 %
<= 0.50 %
Nickel, Ni <= 0.50 %
<= 0.50 %
Other, total 0.20 - 0.50 %
0.20 - 0.50 %
Silicon, Si <= 0.75 %
<= 0.75 %
Descriptive Properties Value Comments
Deep-Drawing Capability rm 1.3 - 1.8
.040 - .070 inches sheet thickness
Strain Hardening Exponent n 0.19 - 0.23
.040 - .070 inches sheet thickness