Mechanical Properties Metric English Comments
Tensile Strength, Yield 375 MPa

@Strain 0.200 %
54400 psi

@Strain 0.200 %
Haynes HR-120® alloy, solution heat-treated
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Tensile Strength, Yield 375 MPa

@Strain 0.200 %
54400 psi

@Strain 0.200 %
Haynes 556® alloy, 0% cold reduction, 1121°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 375 MPa

@Strain 0.200 %
54400 psi

@Strain 0.200 %
Haynes 556® alloy, bar, after 8000 hours at 760°C (1400°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 375 MPa

@Strain 0.200 %
54400 psi

@Strain 0.200 %
Haynes 556® alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 375 MPa

@Strain 0.200 %,
Temperature 95.0 °C
54400 psi

@Strain 0.200 %,
Temperature 203 °F
Haynes Hastelloy® B-3® alloy, 6.3 mm plate
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Tensile Strength, Yield 375 MPa

@Strain 0.200 %
54400 psi

@Strain 0.200 %
Haynes HR-120® alloy, solution heat-treated plate
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Tensile Strength, Yield 375 MPa

@Strain 0.200 %
54400 psi

@Strain 0.200 %
Solution Annealed. Value at room temperature
Special Metals INCONEL® Alloy HX
A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high..