Material Notes:
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencies.Advantages: Torque grades assist flux generation, allowing the motor to develop more mechanical output. If mechanical output is not an issue, permanent magnet or copper winding can be reduced to save on costsApplications: Torque grades are suitable for machines which need high torque at low speeds. They provide the fast acceleration required by hybrid and electric vehicles.Recommendations for use: Torque grades can be used immediately after lamination punching. The effect of punching can be eliminated if a stress relief annealing is applied. This optimises the performance of the Torque grades in applications with fine teeth. It can also provide substantial performance improvements in the lower frequency range. To achieve these effects, a C5 type coating is advised. Torque stacks can be produced using existing assembly techniques such as interlocking or welding.Information provided by ArcelorMittal
Physical Properties Metric English Comments
Density 7.65 g/cc
0.276 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 170 - 200
170 - 200
L direction
170 - 200
170 - 200
T direction
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
490 - 530 MPa
71100 - 76900 psi
T direction
Tensile Strength, Yield 340 - 380 MPa
49300 - 55100 psi
L direction
360 - 400 MPa
52200 - 58000 psi
T direction
Elongation at Break 13 - 28 %
13 - 28 %
L direction
13 - 28 %
13 - 28 %
T direction
Magnetic Properties Metric English Comments
Core Loss <= 18.0 W/kg

@Frequency 400 Hz
<= 8.16 W/lb

@Frequency 400 Hz
at 1T, Guaranteed
<= 41.0 W/kg

@Frequency 700 Hz
<= 18.6 W/lb

@Frequency 700 Hz
at 1T, Indicative
Descriptive Properties Value Comments
Anisotropy >15%
400 Hz at 1T
Polarization >1.55 T
at 2,500 A/m
>1.65 T
at 5,000 A/m
>1.76 T
at 10,000 A/m