Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.1 MPa
6250 psi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 161JA White Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 43.1 MPa
6250 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po..
Tensile Strength, Yield 43.1 MPa
6250 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L9630 Polyvinyl Chloride, Rigid (PVC, Rigid)
Product can meet UL-94V-0. Material passed V-0 @ 1.5mm in screening test at PDI.Information provided by PolyOne
Tensile Strength, Yield 43.1 MPa
6250 psi
ASTM D638
M. Holland Company AB105 ABS
Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Household Goods, Packaging Processing Method: Injection MoldingInformation provided by M. Holland.
Tensile Strength, Yield 43.1 MPa
6250 psi
ASTM D638
I. Stern GPPS-020 General Purpose Crystal Polystyrene
Features:High Strength GradeHigh Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co...
Tensile Strength, Yield 43.1 MPa
6250 psi
ASTM D638
Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene
General Purpose ABS, SD 0150 grade, is a rigid thermoplastic with good processing characteristics. It is a high flow injection molding grade with considerable impact strength and medium heat deflec..
Tensile Strength, Yield 43.1 MPa
6250 psi
ASTM D638
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp
Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..