Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Purpose ABS, SD 0150 grade, is a rigid thermoplastic with good processing characteristics. It is a high flow injection molding grade with considerable impact strength and medium heat deflection.Applications: auto parts, home appliances, electrical parts/fittings, telecommunication and electronic devices.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 1.7 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.7 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 43.1 MPa
6250 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Yield Strength 62.8 MPa
9100 psi
ASTM D790
Flexural Modulus 2.01 GPa
292 ksi
ASTM D790
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525
Flammability, UL94 HB
HB