Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.03 MPa | 1020 psi | ASTM D412 |
Polymax® Maxelast® C4960 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 7.03 MPa | 1020 psi | ASTM D412 |
Polymax® Maxelast® F02-137B TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Strength, Yield | 7.03 MPa | 1020 psi | ASTM D412 |
Polymax® Maxelast® P3660T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 7.03 MPa | 1020 psi | ASTM D412 |
Polymax® Maxelast® P3850 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 7.03 MPa | 1020 psi | ASTM D412 |
Polymax® Maxelast® S4775 TPE, PS Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong .. |
|||
Tensile Strength, Yield | 7.03 MPa | 1020 psi | At 100% elongation, across flow; ASTM D412 |
Advanced Elastomer Systems VistaFlex® 911-B Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Tensile Strength, Yield | 7.03 MPa | 1020 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3080-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength, Yield | 7.03 MPa | 1020 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3311-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 7.03 MPa @Treatment Temp. 200 °C, Time 252000 sec |
1020 psi @Treatment Temp. 392 °F, Time 70.0 hour |
Heat Aging; ASTM D573 |
Vicone High Performance Rubber VicoSil™ 0591EK-CL High Performance Silicone Rubber Information provided by Vicone |
|||
Tensile Strength, Yield | 7.03 MPa @Temperature 21.1 °C |
1020 psi @Temperature 70.0 °F |
Flatwise Tensile |
Hexcel® Redux® 312L Modified epoxy film adhesive Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support.. |
|||
Tensile Strength, Yield | 7.03 MPa | 1020 psi | Flatwise Tensile |
Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 .. |
|||
Tensile Strength, Yield | 7.03 MPa @Temperature 166 °C |
1020 psi @Temperature 330 °F |
Flatwise Tensile; 60 Cycles, Thermal Cycling |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |