Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 53.1 MPa | 7700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 3311-xx23D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ DP-8928-2-8001 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Lucent Polymers GPP-320 Polypropylene, 20% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Lucent Polymers PC/PBT-1212 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Lucent Polymers PC/PBT-1230 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Lucent Polymers PC/PBT-1422 Polycarbonate+PBT, Improved Cold Temp Impact, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Spartech 513 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Spartech 617 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Spartech 829 Static Conductive Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Spartech Spectar® Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Techmer ES HiFill® PBT 1226 Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Techmer ES HiFill® PBT 620 Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS 720 BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS 830 SS7 BK Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Techmer ES Statiblend® PC/ABS 830 SS7 BK with Stainless Steel Fiber Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Styron Pulse® 2000 ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Styron Pulse® 2100LG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM Data |
Styron Pulse® 830 ABS + Polycarbonate PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.PULSE 830 Engineering resin has been used in automot.. |
|||
Tensile Strength, Yield | 53.1 MPa @Thickness 3.20 mm |
7700 psi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can .. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM 638 |
PlastxWorld CEVIAN® S1100 High Impact PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Clariant Renol PA2SP0009HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Clariant Renol PBT1100TF10 Polybutylene Terephthalate, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-20FG-0738 20% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 53.1 MPa | 7700 psi | ASTM D638 |
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F