Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 774 MPa @Temperature 175 °C |
112000 psi @Temperature 347 °F |
Material as cured |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |